Most exterior paint does not peel. It powders. Run a hand down a south facing wall that has gone a few years too long and it comes away chalky, and that chalk is the binder in the paint breaking down under ultraviolet light.
The sun does the damage, not the rain
Florida sits far enough south to get UV levels that northern states see only in midsummer, and it gets them most of the year. UV breaks the resin that holds pigment to the wall. Colour goes flat, the surface goes chalky, and water starts finding its way in.
You can see it in the way a house fails unevenly. The south and west walls go first, often years before the north side looks tired. A house repainted all at once will not age all at once.

The preparation is most of the job
Nothing sticks to chalk, salt film or mildew. The wall gets washed and has to dry properly afterwards, and a block wall holds water longer than it looks. Painting over a damp wall traps that moisture under the film, and it comes back as blisters in the first hot month.
Hairline cracks in stucco get cut out and patched rather than painted over, because paint bridges a crack for one season and then splits along it. Anywhere the old coating has lost its grip has to be scraped back to something sound, and bare or chalky stucco gets primed before any colour goes on.
None of this is visible in a finished photograph. It is the whole difference between a paint job that lasts six years and one that lasts two.
Stucco is its own problem
Stucco is porous and alkaline, and a block wall behind it needs to let moisture out. A coating that seals it completely traps water inside the wall, which is why breathable acrylic systems are the normal choice here and why heavy waterproof coatings can do more harm than good on a house that was never built to be sealed.
Elastomeric coatings are the exception worth knowing about. They are thick and flexible enough to bridge fine cracking, which suits a wall that moves, but they go on heavy and they are unforgiving if the surface underneath was not sound. On the wrong wall they fail in sheets rather than flakes.
Colour is a durability decision
Deep colours fade faster. The pigments that make a rich navy or a strong terracotta are the ones UV attacks hardest, so the darker the wall, the sooner it looks tired. Dark walls also run hotter, which stresses both the coating and the wall behind it.
This is the reason so much of Florida is painted in light, warm neutrals, and it is not only taste. A light body with saturated colour saved for the front door, the shutters and the trim gives you the colour without putting it on the two thousand square feet that take the most sun.
If the house is in a community with an association, check the approved palette before anyone opens a tin.
Exterior painting questions
How often does a Florida house need repainting?
Five to eight years is the usual range for stucco, and the spread inside that range is mostly down to preparation, exposure and colour. A light coloured wall that was properly prepared lasts at the top of it. A dark wall painted over chalk lasts at the bottom.
Can you paint over stucco that is cracking?
Not straight over it. Hairline cracks get opened up and patched first, because paint spanning a crack splits along the same line within a season. Larger or structural cracking is a repair question before it is a painting question, and we will tell you which one you have.
Does washing the house first matter?
It is the single thing most likely to decide whether the job lasts. Salt film, mildew and chalk all stop paint bonding, and none of them are obvious to look at. A wall that was washed and allowed to dry takes paint properly. One that was not is a repaint waiting to happen.